The shale is weathered for 2 years, cream or red
clay
|

The shale is milled or crushed 2mm to
5mm on first level
|
upstairs the crushed shale is mixed with
recycled ash and 5 to 10 % water, then pumped back
downstairs to the presses
|
mixed clay is pumped downstairs to the press,
where bricks are pressed at 40 tons per sq inch,
max 10,000 a day
|
If the brick is to be tumbled, it passes through
the tumbler
|
the bricks are then stacked and stored, ready
for the kiln
|
|